I'm getting only about 5 mounths out of a set of zincs (1988 40' DC). I think I should be getting better than this. We relocated the boat to a temporary location in S.C. recently, and the problem persisted, so apparantly this is not a marina problem. A couple of years ago when I became concerned I had it tested by a surveyor with a background in electrolisis. He said the problem is not the boat. But it's begining to look like the problem may well be the onboard as we have been a transient lately.
Am I wrong to think that I should be getting more than 5 months out of a seto of zincs?
If not, anybody got an ideas what might be the primay culprit?
I have also heard that Hatteras is installing something on all new vessels to minimize this problem (but it's not a galvanic isolator)?
Thanks,
Capt'n Bill
Welcome to the Hatteras Owners Forum & Gallery. Sign Up or Login
Results 1 to 2 of 2
Thread: Zincs
Threaded View
-
06-19-2006 11:14 AM #1
Zincs